Preparation of thermosetting luminescent powder coatings
Raw materialLuminous materialflatting agentepoxyaccelerating agentpolyester resin Preparation methodMix ingredients according to components and contents, add ingredients into a high-speed premixer, mix for 15-20min, then add them into a twin-screw extruder, heat, melt and mix, the heating temperature is 80℃ in zone A and 120℃ in zone B, and… Read More »Preparation of thermosetting luminescent powder coatings